Minghuang ceramic particles

2021/03/17 15:36:03


Directly adding additives into the mixing pot of the mixing plant containing particles can conveniently and quickly produce colored mixtures, eliminating the need for asphalt materials and mineral powder. The production process is similar to that of ordinary asphalt mixtures, and the mixture indicators can meet the requirements of modified asphalt mixtures. When producing the mixture, the temperature of the stone material needs to be between 210 ℃ and 230 ℃, and it takes about 60 seconds to mix. By using this product, all transportation, heating, storage, and energy consumption related to asphalt can be eliminated, and it has the advantages of energy conservation, emission reduction, and environmental protection.


Light gray ceramic particles

Orange ceramic particles